Cross-Linked Silicone Films in Textile Finishing
1967
Welch, Clark M. | Bullock, Joel B. | Margavio, Matthew F.
Dimethyl silicone imparted wrinkle recovery values of 250-285° to various types of fabric when the silicone was cross-linked as a film on the cotton. To enhance this effect, a small amount of cellulose cross-linking was carried out using dihydroxydimethylol ethyleneurea without added metal salt catalysts. Conditioned wrinkle recoveries of 288- 308° and wet recovery angles of 302-310° (W + F) were obtained. The combination treatment has been adapted to durable-press techniques. High crease retention and wash-wear ratings were obtained on sateen after 30-45 machine launderings, with major abrasion damage occurring only after 45 cycles. The application of cross-linked silicone by coating as well as impregnation methods was carried out prior or subsequent to differential (one-sided) cross-linking of fabric: High crease retention and wash-wear ratings after 30 launderings were obtained on twill by this means. Possible effects of these treatments on both the interior and exterior of the cotton fiber are discussed.
اظهر المزيد [+] اقل [-]الكلمات المفتاحية الخاصة بالمكنز الزراعي (أجروفوك)
المعلومات البيبليوغرافية
تم تزويد هذا السجل من قبل National Agricultural Library