Improved Surface Stability of C+MxOy@Na3V2(PO4)3 Prepared by Ultrasonic Method as Cathode for Sodium-Ion Batteries
2017
Klee, Rafael | Wiatrowski, Maciej | Aragón, María J. | Lavela, Pedro | Ortiz, Gregorio F. | Alcántara, Ricardo | Tirado, José L.
Coated C+MₓOy@Na₃V₂(PO₄)₃ samples containing 1.5% or 3.5% wt. of MₓOy (Al₂O₃, MgO or ZnO) have been synthesized by a two-step method including first a citric based sol–gel method for preparing the active material and second an ultrasonic stirring technique to deposit MₓOy. The presence of the metal oxides properly coating the surface of the active material is evidenced by XPS and electron microscopy. Galvanostatic cycling of sodium half-cells reveals a significant capacity enhancement for samples coated with 1.5% of metal oxides and an exceptional cycling stability as evidenced by Coulombic efficiencies as high as 95.9% for ZnO@ Na₃V₂(PO₄)₃. It is correlated to their low surface layer and charge transfer resistance values. The formation of metal fluorides that remove traces of corrosive HF from the electrolyte is checked by XPS spectroscopy. The feasibility of sodium-ion batteries assembled with C+MₓOy@Na₃V₂(PO₄)₃ is further verified by evaluating the electrochemical performance of full cells. Particularly, a Graphite//Al₂O₃@ Na₃V₂(PO₄)₃ battery delivers an energy density as high as 260 W h kg–¹ and exhibits a Coulombic efficiency of 89.3% after 115 cycles.
Show more [+] Less [-]AGROVOC Keywords
Bibliographic information
This bibliographic record has been provided by National Agricultural Library