Delignification of bamboo (Bambusa procera acher). 1. Kraft pulping and the subsequent oxygen delignification to pulp with a low kappa number
2004
Vu, T.H.M. | Pakkanen, H. | Alen, R.
Delignification of bamboo (Bambusa procera acher) was carried out by conventional kraft and soda pulping under varying conditions to determine the relationships between selected cooking parameters (EA 14-20%, sulfidity 0-45%, maximum temperature 165 and 170°C, and time at maximum temperature 30-95 min) and pulp properties (kappa number, viscosity, and yield). Results indicated that in order to obtain relatively low kappa numbers (17-24), high sulfidity (35-45%) at lower EA (14-16%) increased both pulp viscosity and yield compared to the case of low sulfidity (0-15%) at higher EA (16-18%). Pulp with lower kappa numbers (11-15) and acceptable viscosities (1080-1190 ml/g) can be obtained at a sulfidity level of 25-35% with 18% EA or at a sulfidity level of 15-35% with 20% EA. It was further shown that bamboo kraft pulp was easily delignified by oxygen-alkali delignification to a low kappa number (7-9) without any significant loss in viscosity.
Show more [+] Less [-]AGROVOC Keywords
Bibliographic information
This bibliographic record has been provided by National Agricultural Library