Reactivation of Spent FCC Catalyst via Oxidation and Acid Treatment
2020
Abubakar, Abdulkareem | Waba, Ijai Ezekiel | Yunusa, Suleiman | Audu, Nasiru
Reactivation of spent FCC catalyst for its application in the adsorption of heavy metals from wastewater was investigated in this research. The most effective reactivation route of spent FCC catalyst was oxidation of spent FCC catalyst using H2O2 at oxidant-to-catalyst ratio of 16 ml/g, contact time of 60 minutes and a temperature of 90oC, followed by treatment with CH3COOH solution at acid-to-catalyst ratio of 20 ml/g, 75 minutes contact time and at a temperature of 50oC. The reactivation process was monitored using the Scanning Electron Microscope Energy Dispersive X-ray (SEM-EDX), X-ray fluorescence (XRF) and X-ray diffraction (XRD). The result showed significant decreases in impurities of coke and metal, and the crystallinity of the treated spent FCC catalyst was much greater than that of the spent FCC catalyst.
Afficher plus [+] Moins [-]Mots clés AGROVOC
Informations bibliographiques
Cette notice bibliographique a été fournie par Université Ibn Zohr Agadir
Découvrez la collection de ce fournisseur de données dans AGRIS