Modification of Wool by the Application of Linear Synthetic Polyamides
1954
Delmenico, J. | Jackson, D.L.C. | Lipson, M.
Ethanolic potassium hydroxide solutions in concentrations from 0.1% to 5.0% have been used to pretreat wool effectively for the application of N-alkoxymethyl polyamides to prevent felting shrinkage. The alcoholic alkali may be used purely as a pretreatment, or the alkali can be incorporated in the alcoholic resin solution. Even when the alkali pretreatment does not in itself reduce the felting shrinkage, effective shrinkproofing is obtained with less than 1% resin based on the weight of wool.
显示更多 [+] 显示较少 [-]AGROVOC关键词
书目信息
Textile research journal
卷
24
期
9
页码
828
- 834
ISSN
0040-5175
出版者
Sage Publications
其它主题
Textile fibers; Potassium hydroxide
语言
英语
副标题
Part V: Pretreatment with Ethanolic Potassium Hydroxide